Quote:
Originally Posted by stucartwright
Ok... Will post on here.
If you apply the activator to the sticky/non glossy side and therefore stick it to the inside of the shell, that means you are having the best finish on the inside of the shell rather than showing through the shell on the outside. Know what I mean?
I found the dip to be very durable on the outside of the shell.... But inside I'm sure is better.
Would be very interested to hear your thoughts further
|
The process is the same when dipping put sticky side down then dip shell. then relevant base coat. The colour is as good as doing it on the outside if not better as the shine you get from the clear Lexun is really good like I say it's just hard getting it right doing the inside
You should check out pit dawg work look on his web site some cool stuff
This is my current shell