To be fair I think the original ZX5 plastic wasn't the best when it's cold!

Try boiling the plastics for about 10 mins then letting them cool in the water till back at room temp.

Stress relieves the mouldings and makes them more robust.


The later Kyosho plastics (SP / FS) seems to be nearly unbreakable!!!